Preparation : Stir the content thoroughly. On varnished or lacquered wood: Clean with oil thinner and a 00 steel wool. On raw wood: Sand evenly with 120 grit sandpaper and dust off the surface.
Application : Apply a generous oil coat with a stain pad or a cotton rag. After 15 to 30 minutes, remove any excessive oil by rubbing the surface with a cotton rag. Between coats, after 24 hours, perform a slight polish using a 0000 steel wool or an 800 grit sandpaper.
Application tools : Stain pad, Cotton Rag
Number of coats : 3 coats
Drying time :
- Between coats : 24 hours
- Utilization : 2 days
- First damp cleaning : 14 days