Preparation
Mix well before using and use in a well-ventilated area. Sand the raw wood to no higher than 180 grit sandpaper and wipe clean. Remove sanding dust and debris from surface.
Stain if desired, following manufacturer’s directions and dry time.
Application
Brush or apply by wiping on Tung Oil with a clean cloth. Keep surface "wet" for at least 15 minutes to insure penetration into wood pores. Wipe off all excess after a dwell-time of 15 minutes. Allow 24 hours drying. Repeat with a second coat of Tung Oil. Scuff sand between coats with 4/0 steel wool or 320 grit sandpaper. The gloss will increase as more coats are applied. Rub finish to uniform gloss using 4/0 steel wool when finish is dry