Application Temperature:
Above 50°F (10°C)
Open Assembly Time:
5 minutes (70°F./50%RH)
Total Assembly Time:
10-15 minutes (70°F./50%RH)
Minimum Required Spread :
7 mils (typical)
Required Clamping Pressure:
Enough to bring joints tightly together (generally, 30-80 psi for HPL, 100-150 psi for softwoods, 125-175 psi for medium woods and 175-250 psi for hardwoods)
Method of Application:
Easily spread with a roller spreader or brush, or may be transferred to plastic bottles for finer gluing applications.
Cleanup:
Damp cloth while glue is wet. Scrape off and sand dried excess.